22dt Fine Denier Low Melting Point Nylon Hot Fuse

22dt Fine Denier Low Melting Point Nylon Hot Fuse

• 22dt fine-denier bonding yarn
• Low-melting copolyamide material
• Bare-yarn melting point: 85°C
• Composite setting: 105–135°C
• Dry and wet heat processing
• Original white standard color
• 437,333 m per 1,000 g reference
• For weaving and knitting trials
• Related fine-denier sizes available
• Sample testing before bulk orders
Send Inquiry
Product Introduction
Fine-Denier Copolyamide Bonding Yarn
22dt Fine Denier Low Melt Copolyamide Yarn

Fine-denier fusible filament for introducing controlled thermal bonding into woven, knitted or wound textile structures.

22dt grade85°C bare-yarn melting pointDry or wet heat
22dt fine denier low melt copolyamide yarn

22dt Product Data

Use the figures below to plan sampling. Final bonding conditions depend on the substrate, construction, heat-transfer method, pressure and dwell time.

Product grade
22dt fine-denier filament
Material
Low-melting copolyamide adhesive
Bare-yarn melting point
85°C
Composite setting range
105–135°C
Heat method
Dry heat or wet heat
Standard color
Original white
22dt length reference
437,333 m per 1,000 g ±15 g
Related listed sizes
33dt, 44dt, 55dt, 77dt, 111dt
Confirm denier tolerance, package format, color and required quantity before ordering. Conduct a sample trial on the intended textile construction.
fine denier copolyamide yarn for textile thermal bonding

Bonding in Textile Structures

The 22dt filament can be positioned during weaving, knitting or winding. Under controlled heat, the copolyamide softens and creates bonding at the selected area after cooling.

  • Fine placement in lightweight constructions
  • Localized bonding instead of full-area adhesive
  • Compatible with dry- and wet-heat trials
  • Process settings verified on the final substrate

Information for Sample Matching

Provide the construction and processing details needed to evaluate the yarn under representative production conditions.

Textile Structure

Fiber type, fabric construction, yarn placement and the area requiring bonding.

Heat Process

Dry or wet heat, target temperature, dwell time and applied pressure.

Supply Details

Required denier, color, winding format, trial quantity and destination.

Trial Evaluation

Check bond appearance, handling and adhesion after cooling and conditioning.

Frequently Asked Questions

What material is the 22dt yarn?

It is a fine-denier filament made from a low-melting copolyamide adhesive material.

What temperature should be used?

The listed bare-yarn melting point is 85°C and the composite setting range is 105–135°C. Confirm the working setting through trials on the intended materials.

Can the yarn be processed with wet heat?

Yes. Both dry heat and wet heat are listed as acceptable, subject to testing with the selected textile structure.

What is the length reference for 22dt?

The listed reference is 437,333 meters per 1,000 grams with a weight tolerance of ±15 grams.

What should be included in a sample request?

Include the textile structure, heat method, trial conditions, color, winding requirement, quantity and destination country.

Evaluate 22dt Yarn in Your Textile Process

Share the substrate, construction, heat conditions and required quantity.

Request a Sample & Quote

Hot Tags: 22dt fine denier low melt nylon yarn, fine denier copolyamide yarn, 85°C low melt yarn, nylon fusible filament, thermal bonding yarn, copolyamide adhesive yarn, 50D Nylon Hot Melt Yarn, Elastic Nylon Hot Melting Yarn, Nylon Thermal Fuse Yarn, Nylon Hot Melt Yarn Fibers, Nylon Hot Melt Yarn For Shoes Upper, Underwear Fabric Nylon Hot Melting Yarn

(0/10)